适应于大部分塑胶树脂。
通过欧盟及美洲地区ROHS、卤素等多项环保检验合格。在工程塑料体系中有很好的黑度和蓝相。
产品编号 | 载体 | 炭黑含量 | 耐温(℃) | 水分含量(%) | 兼容性 | 建议添加量(%) | 环保标准 |
2014H | LLDPE, | 55% | 120-300℃ | ≤0.1% | PE,PP,ABS,PS,PC,PA,POM,PBT | 1-3% | ROHS,卤素 |
2014G | LLDPE | 52% | 120-300℃ | ≤0.1% | PE,PP,ABS,PS,PC,PA,POM,PBT | 1-3% | ROHS,卤素 |
2014E | LLDPE | 50% | 120-300℃ | ≤0.2% | PE,PP,ABS,PS,PC,PA,POM,PBT | 1-3% | ROHS,卤素 |
2014C | LLDPE | 47% | 120-300℃ | ≤0.2% | PE,PP,ABS,PS,PC,PA,POM,PBT | 1-3% | ROHS,卤素 |
2014B | LLDPE | 45% | 120-300℃ | ≤0.2% | PE,PP,ABS,PS,PC,PA,POM,PBT | 1-3% | ROHS,卤素 |
2014 | LLDPE+PE | 43% | 120-300℃ | ≤0.2% | PE,PP,ABS,PS,PC,PA,POM,PBT | 1-3% | ROHS,卤素 |
7088 | PE | 43% | 120-300℃ | ≤0.3% | PE,PP,ABS,PS,PC,PA,POM | 1-3% | ROHS,卤素 |
7086 | PE | 41% | 120-300℃ | ≤0.3% | PE,PP,ABS,PS,PC,PA,POM | 1-3% | ROHS,卤素 |
7080 | PE | 38% | 120-300℃ | ≤0.3% | PE,PP,ABS,PS,PC,PA,POM | 1-3% | ROHS,卤素 |
7066 | PE | 32% | 120-300℃ | ≤0.3% | PE,PP,ABS,PS,PC,PA,POM | 1-3% | ROHS |
7063 | PE | 34% | 120-300℃ | ≤0.3% | PE,PP,ABS,PS,PC,PA,POM | 1-3% | ROHS |
7060 | PE | 36% | 120-300℃ | ≤0.3% | PE,PP,ABS,PS,PC,PA,POM | 1-3% | ROHS |
7301 | PP | 28% | 120-300℃ | ≤0.3% | PE,PP,ABS,PS,PC,PA,POM | 1-3% | ROHS |
7056 | PP | 25% | 120-300℃ | ≤0.3% | PE,PP,ABS,PS,PC,PA,POM | 1-4% | ROHS |
7030 | 改良复合树脂 | 28% | 120-300℃ | ≤0.3% | PE,PP,ABS,PS,PC,PA,POM | 1-4% | ROHS |
6040 | 改良复合树脂 | 25% | 120-300℃ | ≤0.3% | PE,PP,ABS,PS,PC,PA,POM | 1-4% | 未测试 |
6013 | 改良复合树脂 | 20% | 120-300℃ | ≤0.3% | PE,PP,ABS,PS,PC,PA,POM | 1-4% | 未测试 |
6009 | 改良复合树脂 | 12% | 120-300℃ | ≤0.3% | PE,PP,ABS,PS,PC,PA,POM | 1-6% | 未测试 |
6003 | 改良复合树脂 | 9% | 120-300℃ | ≤0.3% | PE,PP,ABS,PS,PC,PA,POM | 1-6% | 未测试 |
6002 | 改良复合树脂 | 5% | 120-300℃ | ≤0.3% | PE,PP,ABS,PS,PC,PA,POM,TPU,TPR | 1-6% | 未测试 |